Chemical Composition: C: 0.32–0.45%, Cr: 4.75–5.50%, Mo: 1.10–1.75%, Si: 0.80–1.20%, Mn: 0.20–0.60%, V: 0.80–1.20%, P/S ≤ 0.030%, rest Fe
Key Benefits: Balances strength and toughness (no chipping); resists heat and fatigue; stays strong in high temperatures
Hardness: HRC 50–55
Best For: Hot cutting, thick blades, high-impact rebar, heavy-duty continuous cutting (e.g., high-strength rebar)
Hard and wear-resistant (better than regular alloy blades)
Good for cutting hard cold-rolled rebar
Note: Less tough—avoid high-impact, large-gap cutting (may chip)
Affordable and easy to use
Good for cutting ordinary low/medium-strength rebar
Ideal for small/medium construction projects (saves cost)
Square blades: 4 usable edges (rotate to extend life); for large-scale continuous cutting
Rectangular blades: 1 or 2 edges; for small-tonnage machines (not for heavy duty)
Circular blades: For special dedicated cutters
Machines like GQ40, GQ50, GQ60 have fixed standards for blade thickness, length, width, and bolt hole spacing
Follow your machine’s manual—wrong size hurts cutting quality and damages the machine
Fits global brands (Peddinghaus, Geka, etc.)
Ordinary round steel: Low hardness; 9CrSi or Cr12MoV is enough (saves cost)
High-strength ribbed rebar (HRB400/500): Hard with ribbed surface (wears blades); use H13 (resists wear and chipping)
Also works for flat steel, square steel, and other metal profiles
All AlasMachinery blades use full precision grinding and vacuum heat treatment
Vacuum heat treatment: Uniform hardness (HRC 56-62) – no soft spots (avoids quick wear)
CNC grinding: Exact size, fits machines perfectly, reduces vibration (no chipping/blunting)
Clean, flat 90-degree cuts every time
Solves brittle fracture when cutting high-strength rebar
Optimized hardness and toughness for heavy-duty use
Fits standard and special cutting needs
Poor blades cause problems: More machine strain (damages motors/gears), uneven cuts (hard to weld), safety risks (blades may shatter)
High-quality blades save time, money, and keep workers safe
We make cutting solutions (not just blades)
Premium materials, strict quality control, and perfect compatibility
Blades work well in extreme industrial conditions
Adjust the gap between moving and fixed blades based on bar diameter
Rotate square blade edges before they go dull
Use high-strength bolts and check their tightness daily (prevents blade shake)
In-stock inventory for fast global shipping
No delays to your project
Maximizes your return on investment (ROI)
| NO. | Product Name | Specification Dimensions (length x width x height/thickness) ) | Material | Remarks |
| 1 | bar cutter blade size | 78*78*17 mm | H13 | Customization services are available; we can manufacture according to your drawings, with a minimum order quantity of 2 piece. |
| 2 | 80*80*17 mm | |||
| 3 | 80*80*30mm | |||
| 4 | 83*83*16 mm | |||
| 5 | 83*83*26 mm | |||
| 6 | 83*83*26 mm | |||
| 7 | 90*90*20mm | |||
| 8 | 90*90*26 mm | |||
| 9 | 100*100*20mm | |||
| 10 | 100*100*30 mm | |||
| 11 | 110*110*20 mm | |||
| 12 | 100*30*75 mm | |||
| 13 | 85x65x30 mm | |||
Base Grade | Steel Category | Chinese Standard GB/T 1299 | American Standard ASTM | German Standard DIN (W-Nr.) | Japanese Standard JIS |
| H13 | Hot Work Die Steel | 4Cr5MoSiV1 | H13 | 1.2344 | SKD61 |
Cr12MoV | Cold Work Die Steel | Cr12MoV | 1.2601 | SKD11 | |
9CrSi | Alloy Tool Steel (Cutting Tool Steel) | 9CrSi | 1.2108 |





English: Bar Cutter Blade | Steel Bar Shearing Knives
French (Français): Lame de coupe-barre | Couteaux pour cisaille à barres
Portuguese (Português): Lâmina de corte de barra | Facas para cisalha de barras de aço
Polish (Polski): Nóż do cięcia prętów | Noże do nożyc do prętów stalowych
Turkish (Türkçe): Çubuk Kesme Bıçağı | Çelik Çubuk Makas Bıçakları
Vietnamese (Tiếng Việt): Lưỡi dao cắt thanh thép | Dao cắt thép thanh tròn
Thai (ภาษาไทย): ใบมีดเครื่องตัดเหล็กเส้น | ใบมีดสำหรับตัดแท่งเหล็ก
Filipino: Blade ng Bar Cutter | Mga Kutsilyo para sa Pagputol ng Baras na Bakal
Arabic (العربية): شفرة مقص قضبان الحديد | سكاكين قص قضبان الصلب
Hindi (हिन्दी): बार कटर ब्लेड | स्टील बार शीयरिंग चाकू
Indonesian (Bahasa Indonesia): Pisau Pemotong Batang Besi | Bilah Shearing Batang Baja
Malay (Bahasa Melayu): Bilah Pemotong Bar Keluli | Pisau Gunting Bar Keluli
Dutch (Nederlands): Staven snijblad | Messen voor staalstaf scharen
Swedish (Svenska): Stångklippblad | Knivar för stångklippning
Hungarian (Magyar): Rúdvágó penge | Acélrúd nyíró pengék
Greek (Ελληνικά): Λεπίδα κοπής ράβδων | Μαχαίρια ψαλιδιού χαλύβδινων ράβδων
Based on different working conditions and budget requirements, we offer three general industrial-grade alloy steel materials:
9CrSi (Alloy Tool Steel): An economical choice. It has good hardenability and machinability, suitable for cutting ordinary medium-to-low strength rebar, and is widely used in small and medium-sized projects.
Cr12MoV (Cold Work Die Steel): High-end wear-resistant type. High carbon and high chromium content, after heat treatment, it has excellent wear resistance, making it an ideal choice for continuous cutting of high-strength rebar. Its service life is much longer than 9CrSi.
H13 (Hot Work Die Steel/Red Hard Steel): High toughness and high wear resistance. It exhibits excellent resistance to chipping and thermal stability in rebar cutting applications, especially suitable for high-speed production lines or online cutting of hot-rolled rebar, and cutting of ultra-thick rebar and composite materials of scrap rebar.
Chipping is usually caused by the following factors:
Insufficient toughness: Using ultra-hard but low-toughness materials to cut large-diameter or ultra-hard rebar can easily lead to brittle fracture. In this case, we recommend switching to H13 material, as its excellent toughness can effectively absorb impact forces.
Improper clearance: Too large or too small a gap between the upper and lower blades will lead to uneven stress, resulting in chipping.
Insufficient heat treatment: Internal stress is not completely eliminated. All our blades use vacuum heat treatment technology to ensure uniform hardness from the inside out, greatly reducing the chipping rate.
For high-strength or ribbed rebar, we strongly recommend H13:
If you are facing extremely high operating intensity and are concerned about downtime due to blade chipping, choose H13. Its impact fatigue resistance is top-notch in the rebar processing industry.
Yes. We understand that blade specifications vary among different equipment brands (e.g., from Italy, Germany, or China). We are equipped with a full set of CNC machining equipment, and you only need to provide the following information:
Detailed drawings (including length, width, thickness, and hole dimensions).
Material requirements (9CrSi, Cr12MoV, or H13).
Specifications of the workpiece to be processed (rebar diameter and strength grade).
We can provide a 1:1 precise customized solution.
Regular rotation: Our blades are usually designed with 4 or 8 cutting edges. Please rotate the blade promptly when one cutting edge becomes dull.
Tighten bolts: Ensure the blades are securely installed. Any slight looseness will cause destructive impact during the cutting process.
Control the gap: Adjust a reasonable blade gap according to the rebar diameter, usually about 10% of the rebar diameter.
Nanjing Alas International Co., Ltd. is a professional industrial tooling manufacturer focused on shear blades, bending dies, shredder blades, and custom wear parts. We offer full application engineering, material selection, setup guidance, and after-sales support to global customers.
Tell us your requirements, and our engineering team will provide professional solutions for blade specification, tool life optimization, and cost-effective production.